dc.description.abstractAn electrochromic window was fabricated by combining polyaniline and tungsten oxide with a solid polymer electrolyte binding the two electrochromic materials together. Polyaniline and tungsten oxide were deposited electrochemically on indium-tin-oxide glass plates. By applying a voltage between −1800 and +1600 mV, the transmission spectra for the electrochromic window show good light modulation in the 400–2700 nm wavelength region. For example, at 1000 nm the transmission changes from 0.76 to 0.22.nb_NO
dc.language.isoengnb_NO
dc.publisherElseviernb_NO
dc.titleTransmission Spectra of an Electrochromic Window based on Polyaniline, Tungsten Oxide and a Solid Polymer Electrolytenb_NO
dc.typeJournal articlenb_NO
dc.typePeer reviewednb_NO
dc.description.versionacceptedVersionnb_NO
dc.source.pagenumber1377-1380nb_NO
dc.source.volume37nb_NO
dc.source.journalElectrochimica Actanb_NO
dc.identifier.doi10.1016/0013-4686(92)87010-W
dc.identifier.cristin358676
dc.description.localcodeThis article will not be available due to copyright restrictions (c) 2001 by Elseviernb_NO
cristin.unitcode194,66,35,0
cristin.unitnameInstitutt for materialteknologi
cristin.ispublishedtrue
cristin.fulltextoriginal
cristin.qualitycode2


Files in this item

Thumbnail

This item appears in the following Collection(s)

Show simple item record